Reading a joint failure
Where the break runs tells you what caused it: the glue, the timber, the design or the guest.
Four patterns
Clean separation with glossy surfaces is a starved joint or a glue that never cured. Timber failure beside the joint means the glue held and the section was too small. The crack running through a knot is the timber. The joint that has opened without breaking is creep or moisture.
Each points at a different fix, and three of the four are the factory's.
What to photograph
The joint opened up, the broken faces in raking light, and a tape measure across the section. Those three images let a factory answer without a site visit, and they are what a claim needs.
Frames that survive the first two years usually go on to survive ten, which is the pattern on hotel dining chairs.
When to replace rather than repair
If the timber beside the joint has failed, a repair is holding a smaller section than the design allowed. Replace the frame. If the joint opened cleanly, a re-glue with epoxy and a clamp will outlast the chair.
This is in the joinery guide, with repair or replace a joint and joint creep in service as the two notes that follow.
Table frames that fail at the apron bolt are under hotel dining tables.