Craft Notes
Home · Timber

Density is not strength

A heavier timber is not automatically a stronger chair. Density predicts wear at a surface; strength lives in the section.

21 Nov 2026 · Timber
The guide behind thisThe timber guide: which species belongs on which part of a chair — Eight species by density, Janka and movement, and the part of the frame each one should be on. Start from the load, not from the look.

What density does predict

Density tracks hardness and abrasion resistance fairly well, which is why it is a decent proxy for how a leg wears at the floor contact and how a top takes a dropped plate. It tracks bending strength much less well, because bending strength depends on the section and the grain direction, not on mass.

The 700 kg/m³ beech leg at 32 mm square is stronger than a 750 kg/m³ oak leg at 26 mm square. The species is heavier and the chair is weaker. Nobody reading a specification sheet would guess that, which is why the section goes on the sheet too.

Where the section is decided

Legs, rails and back posts are sized by the drawing, and the drawing is usually copied from a chair the designer liked. That is how 26 mm legs get specified for a room that needs 32 mm. The fix is not a harder species; it is 6 mm more section, which costs less than the upgrade.

The same logic applies to seat rails: depth carries the joint, thickness carries the load. The 60 mm deep rail with a 30 mm tenon beats a 40 mm rail in oak with a 25 mm tenon. Frames drawn to a section are grouped under hotel dining chairs.

The two questions

Ask what the timber is, and ask what the section is. The supplier who can answer both is working from a drawing; one who answers only the first is working from a photograph.

This is the core of the timber guide. The notes that follow it are beech or oak and Janka and a dropped plate.

The heavier tops where this matters most are on hotel dining tables.