Three glues, three failure modes
PVA, PU and epoxy are not interchangeable, and the wrong one fails in a way that looks like bad workmanship.
PVA
Cross-linked PVA (D3) is the default for interior joints: strong, cheap, water-resistant enough for a dining room and easy to clean up. It creeps under sustained load, which matters on a bent lamination and not much on a chair rail.
It also fails at about 60 °C, which is why a chair left in a hot container for a month can arrive with open joints that were sound when they were packed.
PU and epoxy
PU foams slightly as it cures, fills a small gap and survives damp. It is the right choice for teak and for anything that may see weather, and the wrong choice where the joint line will be visible, because the foam shows.
Epoxy fills a real gap and is the repair adhesive, not the production one. Frames glued with the correct adhesive for their end use are on hotel dining chairs.
The specification line
Name the glue by class, not by brand: D3 PVA for interior frames, PU for anything that may see damp. That is enough for a factory to work to and enough for you to check.
More in the joinery guide, with glue line thickness and clamping time and cure as the related notes.
Outdoor-adjacent frames, glued in PU, are under hotel dining chairs.