Knots: where one is a defect and where it is free
A knot in a leg is a crack waiting for a load. A knot in a painted panel is character nobody will ever see.
Why a knot fails
The knot is a branch that grew at an angle to the grain. The fibres around it turn, so the section that carries load is smaller than the outside dimension suggests. Under bending, the crack starts at the edge of the knot and runs with the grain, which is why a knot near a mortise is worse than a knot in the middle of a rail.
Under compression, a knot in a leg is less dangerous. Under tension, as in the underside of a bent back, it is the first thing to go. Same defect, different verdict, depending on which part of the chair it lands in.
Where to allow them
Painted panels, internal rails, the underside of a seat frame: anywhere out of sight and out of tension. Nowhere on a visible leg, a back post, an arm, or any part that is steam bent.
The size limit matters too. Anything over 15 mm across on a visible face is a rejection on most contract specifications; 8 mm is the usual allowance on second-grade stock. Frames sorted to that rule are on hotel dining chairs.
Writing the clause
One line does the work: no knots on visible faces, knots under 15 mm allowed elsewhere. It is short, checkable, and it does not push the price up much, because the factory is already sorting for its own yield.
The species context is in the timber guide, next to sapwood in a frame and end grain and water.
The panels where a knot is harmless are described under booth seating.