Rust spots at the floor contact, and why they come back
The spot is the symptom. The water sitting inside the tube is the cause.
The mechanism
Water enters at the glide socket and sits in the bottom 20 mm of the leg, where there is no airflow and no coating. 1.2–1.5 mm steel rusts through from the inside in about three wet seasons.
The prevention is in powder chip treatment, and the outdoor case is in rust at the floor contact.
What to do
Sand to bare metal, treat with a conversion coat, touch in with a two-pack repair paint. Sealed plugs in the foot stop the water getting back in.
Frames with sealed feet and stainless hardware are on hotel dining chairs, and the stainless case is in stainless where it is worth it.
When it is structural
If a probe goes through the wall, the leg is gone. Rust through a 1.2 mm wall at the foot is a replacement, not a paint job.
This is in the care guide, with powder chip treatment as the note on stopping it earlier.
Outdoor and poolside frames carry the risk, and the sealed-foot versions are on hotel dining chairs.