A chipped powder coat is a rust start, not a cosmetic mark
The coat is 60–80 micron. A 5 mm chip exposes bare steel to every wipe.
Why it spreads
Rust under a powder coat creeps sideways under the film, so a 5 mm chip becomes a 20 mm blister in a year. 60–80 micron, cured at 180–200 °C is thin enough that the creep is invisible until it lifts.
The repair sequence is in rust spot treatment, and the factory prep that prevents most of it is in metal prep before powder.
The field repair
Clean, dry, two-pack touch-in paint in the matched colour, two coats. It is visible at 300 mm and invisible at a metre, which is the standard a hotel should hold itself to.
Matched colours and spare paint are supplied with hotel dining chairs, and the on-site version is in powder touch up on site.
The cause to fix
Chips come from stacking and from trolleys, not from guests. Line the trolley and change the stacking practice, or the same chair chips again in a month.
This is in the care guide, with bleach and ammonia damage as the note on the chemical version of the same problem.
Touch-in paint is supplied in the matched colour with the order, and the ranges are on hotel dining chairs.