Veneer lifts at the edge, never in the middle

An unlipped veneered top fails within a season of trolley traffic, and it fails where nobody can fix it.

20 Nov 2026 · Finish
The guide behind thisThe finishing guide: lacquer, oil, veneer, laminate and stone — Five surfaces, what each one does under a hot plate and a cleaning trolley, and the re-finish interval you are actually committing to.

Why the edge

0.6 mm sliced veneer on 18 mm board, edges lipped in solid. The edge is where the veneer ends, where moisture gets in, and where a trolley hits. Once the veneer lifts by a millimetre, it cannot be glued back invisibly.

The solid lipping moves the failure somewhere it can be sanded and refinished.

What lipping costs

One more machining operation and a strip of solid timber per edge. On a 750 mm top that is a few dollars, and it is the difference between a top that lasts and one that gets replaced.

Lipped tops are standard on the hotel dining tables range.

The delivery check

Run a fingernail along the edge. Any catch or hollow sound is a veneer that is already lifting, and it will not improve in a heated room.