Craft Notes
Home · Finish

Finish

Lacquer, oil, veneer, laminate and stone — how each ages in a dining room.

Read the the finishing guide: lacquer, oil, veneer, laminate and stone first — it holds the numbers these notes work from.

Distressed finishes in a contract room

A deliberately worn finish hides real wear, until the real wear lands somewhere the pattern did…

Three edge bands, three lifetimes

PVC, ABS and solid timber lipping behave differently under a chair leg and a…

Shipping a finish before it cures

A lacquered frame packed on the day it was sprayed arrives with the carton printed into the…

The sample finish is not the production finish

A sample room sprays a part by hand. A production line sprays a batch. The two are the same recipe and a…

Glass tops scratch, and you cannot fix it

Toughened glass is strong in the middle and fragile at the edge. A chip there means the whole top…

Sheen level decides how a finish wears

A matt finish hides scratches and shows fingerprints. A gloss finish shows every mark and cleans…

Laminate where water lives

An HPL top survives a buffet counter and a mop. A lacquered timber top does…

Matt, satin or gloss: what the room does

The light in the room decides the sheen more than the design intent…

Moisture under the film

Spray a part at 12% and seal it in, and the moisture stays there until the film cracks or a joint…

Oil finishes and the twelve-month cycle

An oiled top can be repaired by anyone with a cloth. It also needs that cloth every…

Open pore or closed pore

A filled pore looks like plastic and wipes clean. An open pore feels like timber and collects whatever is…

Paint chips at the edge, always

A painted frame survives a busy room if the edge was primed and the corner has a radius. Without both, it chips…

Reactive stain on oak, and the patch that shows

It colours the timber by reacting with the tannin, so a repair cannot be tinted to…

Swirl marks under a low light

A top finished too fast looks perfect at noon and covered in circles at eight in the…

The sanding between coats is the finish

Three coats sprayed wet-on-wet is one coat with two shadows of orange peel in…

Solid surface for a buffet counter

It can be sanded back to new, joined invisibly and shaped without a joint. It also…

Stone edge profiles and the chipped corner

A square edge chips at the first chair back. A 3 mm radius chips less and looks the same from standing…

A stone top changes the table underneath

Twenty millimetres of granite adds 25–35 kg to a four-top. The base, the glides and the way staff move it all…

Tinting, and why two batches never match

A toner in the lacquer is what makes three species look like one. It is also what makes a second order…

Touch-up pens fix a scratch, not a finish

They are colour, not film. On a matt surface the colour matches and the sheen does…

Two-pack lacquer and the older nitrocellulose

One resists a hot plate and a cleaning trolley. The other is what a workshop uses when it wants a fast…

UV-cured finishes, and where they stop

Cured in seconds under a lamp, hard as a laminate, and impossible to repair…

Veneer lifts at the edge, never in the middle

An unlipped veneered top fails within a season of trolley traffic, and it fails where nobody can fix…

Water-based lacquer in a hotel

Lower solvent, softer film. It is the right choice for a room that has to open the week after…

Wax is not a finish

It is a maintenance layer over a finish. On bare timber it does nothing except attract…