The setting

a 1.2 mm wall takes 60–70 A; above that the tube blows through. Turn it up to weld faster and the tube blows through, which the welder fills with a patch. The patch cools faster than the surrounding metal, leaves a stress riser at its edge, and the frame cracks next to the weld rather than at it.

That crack is the one that appears above the front leg on a frame that has been in service for a year, and it is almost never diagnosed as a welding fault.

What a good weld looks like

The 360° fillet with a consistent bead, no undercut at the toe, ground flush before powder. Grinding hides a lot, which is why the check happens before the grinder rather than after.

Frames that pass are on hotel dining chairs, and the same weld standard applies to the steel under counter stools.

The check

Look at the inside of a joint where the grinder cannot reach. The bead that runs around the tube on the outside and stops on the inside is a half-welded joint that will fail in fatigue.

The process is in the joinery guide, with welded versus bolted and metal prep before powder as the follow-on notes.

Steel-framed tables are under hotel dining tables.