Craft Notes
Home · Metal

Powder does not stick to a dirty frame

Four stages before the spray, and skipping one shows up as rust at the weld seam in eighteen months.

24 Nov 2026 · Metal
The guide behind thisThe metal guide: wall thickness, welds and the salt spray number — Why 1.2 mm and 1.5 mm are different chairs, where rust starts on a welded frame, and what a 500 hour salt spray result actually proves.

The four stages

degrease, rinse, conversion coat, dry — four stages. Each stage has a job: degrease removes drawing oil, rinse removes the cleaner, conversion coating keys the surface, dry removes the water that would flash-rust in the oven.

Skip the conversion coat and the powder sits on bare steel with nothing bonding it. It looks perfect and lifts in sheets.

Where it goes wrong

At the weld seam, where flux residue and mill scale sit in a crevice the wash cannot reach. The powder covers it, the rust starts underneath, and the first sign is a bubble at the seam.

Frames that pass a 500-hour salt spray coupon are on hotel dining chairs, and the same prep applies to steel under counter stools.

The check

Ask for the coupon result and the film thickness, not just the process name. 60–80 micron over a conversion coat is a specification; "powder coated" is a description of a colour.

This is in the metal guide, with weld quality and powder thickness and edges as the follow-on notes.

Steel table frames are under hotel dining tables.