Craft Notes
Home · Timber

Laminated curves, and why they are stronger

Eight thin plies beat one bent stick, and the reason is in the glue lines rather than the timber.

28 Nov 2026 · Timber
The guide behind thisThe timber guide: which species belongs on which part of a chair — Eight species by density, Janka and movement, and the part of the frame each one should be on. Start from the load, not from the look.

The mechanics

Each ply carries the bend in the same direction and the glue line stops a crack from running through the section. The solid bent part is one piece of timber with a stress gradient through it; a laminate is eight thin pieces, each with a fraction of that stress.

That is why a laminated back post survives a load that splits a solid one at the same radius. It is also why the laminate weighs the same and costs more labour: cutting, spreading glue, pressing and cleaning up eight plies takes longer than clamping one bent blank.

Where the ply count matters

Three plies is a bent board. Eight to twelve is a structural curve. The factory quoting six plies for a 200 mm radius back post is quoting a part that will delaminate at the outside face where the ply is stretched thinnest.

Ask for the ply count and the glue type. Cross-linked PVA is fine indoors; anything that may see damp needs PU. Laminated frames are listed with the hotel dining chairs.

The visible edge

The laminated part shows glue lines on the edge, and they read as stripes under a clear finish. If the design wants a clean edge, the part is lipped in solid, which is another process and another price. Under an opaque finish none of this matters, which is why painted frames use laminates freely and clear-finished ones do not.

This is covered in the timber guide, with steam bending limits and mixing species as the related notes.

Solid-lipped tops are under hotel dining tables.