Where steam bending stops working

Under 200 mm radius the failure rate climbs fast, and no amount of skill makes a bent stick behave like a laminate.

28 Nov 2026 · Timber
The guide behind thisThe timber guide: which species belongs on which part of a chair — Eight species by density, Janka and movement, and the part of the frame each one should be on. Start from the load, not from the look.

The limits by radius

At 400 mm and above, most species bend reliably. Between 300 and 400 mm, ash and beech work with a good form and a controlled springback. Below 200 mm, the outside of the bend starts to rupture on a regular share of blanks, and the rejects go in the bin rather than the price.

The failure is tension on the outside face. Steam plasticises the lignin but it does not add fibre, so a tight radius asks the outside to stretch more than the cells allow. The blanks that survive look fine and fail later, which is the expensive half of the problem.

What the alternatives cost

The laminated curve has no reject rate worth mentioning, holds a tighter radius and is dimensionally stable. It costs more in labour: cutting plies, gluing, pressing, cleaning up. For a run of 200 chairs the labour is spread thin, and the laminate wins on both cost and consistency.

Solid bent parts are honest on a generous radius, and they show end grain on the face, which some designs want. Bent frames are part of the hotel dining chairs range.

What to ask the sample room

Give the radius and the quantity, and ask what the reject rate is on that radius in that species. The straight answer tells you the sample room has done it before; a vague one tells you the first batch is the experiment.