The sanding between coats is the finish

Three coats sprayed wet-on-wet is one coat with two shadows of orange peel in it.

31 Dec 2026 · Finish
The guide behind thisThe finishing guide: lacquer, oil, veneer, laminate and stone — Five surfaces, what each one does under a hot plate and a cleaning trolley, and the re-finish interval you are actually committing to.

The sequence

Sealer, sand 320, first top coat, sand 400, second top coat, de-nib 600. two-pack polyurethane, 3 coats, 30–40 micron dry film, 24 h between coats The sanding is what removes the grain raise the sealer caused.

The grain raise is in sanding and surface prep, and the swirl marks it leaves are in sanding grit and swirl marks.

What skipping it looks like

The surface that is glossy and slightly rippled, visible at a low angle across a tabletop. Guests read it as cheap and it is the first thing a buyer notices under a window.

Finishes built coat by coat are on dining table tops, and the booth side is in spray booth and finishing.

The dry film

30–40 micron total, measured on a test panel from the same run. Below 25 micron the finish wears through at the front edge in a year.

This is in the finish guide, with open pore versus closed pore as the note on how much of that film is visible.

Sealer and two top coats is the minimum that survives a dining room, and the models are on contract dining chairs.