A lifted veneer edge gets worse every time it is wiped
Water wicks under the 0.6 mm slice and the cloth catches the lip. Two wipes and it is gone.
Why it lifts
0.6 mm sliced veneer on 18 mm board, edges lipped in solid The edge is the weakness, and a damp cloth dragged across it lifts the slice about 0.2 mm every pass.
The edge detail that survives it is in veneer edge lifting, and the banding choice is in edge banding types.
The repair
Inject PVA under the lift with a syringe, press with a heated block for 60 seconds, then clamp for two hours. Without heat the veneer cracks along the grain.
Tops with a solid lipping rather than a taped edge are on hotel dining tables, and the humidity that starts the lift is in humidity band in a dining room.
The stopping point
Once the veneer has curled past 20°, it will not lie flat without splitting. That is a new top or a re-laminate, and both are cheaper than a third repair.
This is in the care guide, with cleaning agent pH as the note on the cloth that caused it.
Veneered chair backs lift at the same edge, and the lipped versions are on hotel dining chairs.