Craft Notes
Home · Metal

Chrome pits, and it starts at a scratch

A 0.2 micron scratch through the chromium lets moisture reach the nickel, and the pit grows from underneath.

22 Nov 2026 · Metal
The guide behind thisThe metal guide: wall thickness, welds and the salt spray number — Why 1.2 mm and 1.5 mm are different chairs, where rust starts on a welded frame, and what a 500 hour salt spray result actually proves.

The mechanism

Chromium is decorative and porous at a microscopic scale. Once moisture reaches the nickel layer, the two metals form a small cell and the nickel corrodes, lifting the chrome above it.

That is why a chrome frame in a wet area looks fine for a year and then shows white spots that cannot be cleaned off.

Where it happens

Floor contacts, footrests, and anywhere a trolley hits. Chlorinated cleaners accelerate it, so a poolside chrome frame is the worst case.

Wet areas are better served by stainless or powder, which is why the counter stools in buffet zones are usually powder. It is also why a chrome frame in a poolside shower area is a decision nobody repeats twice.

If you already have chrome

Wipe dry after cleaning and avoid abrasive cream. The wax coat slows it. There is no repair once pitting starts, only replacement of the part.

This is in the metal guide, next to chrome versus powder and metal and cleaning chemicals.

Chrome table bases in dry rooms are under hotel dining tables.