Craft Notes
Home · Metal

Metal

Wall thickness, welds, powder and the salt spray number behind them.

Read the the metal guide: wall thickness, welds and the salt spray number first — it holds the numbers these notes work from.

Aluminium frames are light, and that is the problem

A chair that weighs 3.5 kg is easy to move and easy to tip. The fix is in the splay, not the…

Brass, bronze and the patina argument

Lacquered brass stays gold until the lacquer wears, then it patches. Unlacquered brass goes brown and stays…

Chrome pits, and it starts at a scratch

A 0.2 micron scratch through the chromium lets moisture reach the nickel, and the pit grows from…

Chrome or powder: the honest comparison

Chrome reflects a room and shows every fingerprint. Powder takes colour and hides wear until it…

Fixing a timber top to a steel base

Steel does not move and timber does. Screw them together rigidly and the top splits in the first dry…

Folding mechanisms and the hinge that goes first

A folding chair is a machine with one moving part, and that part is where every complaint…

The footrest is where a stool dies

A guest rests a heel there for an hour, twice a day, for years. No other part of a stool takes…

Glides, floors and the wrong 8 mm

A felt glide protects a wooden floor and wears out in a season. Nylon lasts and marks a soft…

What cleaning chemicals do to a metal frame

Bleach dulls powder, ammonia attacks aluminium, and an abrasive cream removes the coating before it removes the…

Powder colour fades, and warm colours fade first

A south-facing window will move a red frame toward orange in three years. Black will move toward…

Powder does not stick to a dirty frame

Four stages before the spray, and skipping one shows up as rust at the weld seam in eighteen…

How a metal frame holds a seat

Welded lugs, a wire frame or a plate. Each one decides how the seat pad sits and how long it…

Powder is thinnest where rust starts

The gauge is pointed at a flat face. The edges and holes carry two thirds of that film, and that is where…

Touching up powder on site

A 20 mm chip on a leg is visible from three metres. An aerosol and ten minutes makes it disappear for a…

Rust starts at the floor line

The bottom 20 mm of a steel leg is wet more often than any other part of a chair, and it is the part nobody…

Salt spray proves the process, not the chair

Five hundred hours on a flat coupon is a process check. It says nothing about a crevice the coupon does not…

Where stainless is worth the price

In a wash-down room it pays for itself in two years. In a dining room it is money spent on a look nobody asked…

How much base a stone top needs

A 20 mm stone top on a 750 mm four-top adds 25–35 kg. The base has to carry that and not…

When a steel frame gets cheaper, the wall gets thinner

Steel is a commodity and a frame has a fixed shape. The only variable a factory can cut without redrawing is…

What 1.2 mm steel actually means

Two frames look identical in a photograph and differ by a third in steel. The difference shows at the footrest,…

Threads in metal, and the one that strips

An M8 thread in a 1.2 mm tube has two and a half turns of engagement. That is not enough to hold a…

Round, square or oval: the tube shape question

A square tube resists bending better per kilo. A round tube resists twisting better and looks…

Welded or bolted: choosing a metal frame

A weld is permanent and a bolt is a maintenance item. Both are right, in different…

Welded leg or cast base

A cast base is heavier, quieter and impossible to repair at the leg. A welded one is repairable and…

Welding pulls a frame out of square