Home · Metal

Powder is thinnest where rust starts

The gauge is pointed at a flat face. The edges and holes carry two thirds of that film, and that is where corrosion begins.

25 Nov 2026 · Metal
The guide behind thisThe metal guide: wall thickness, welds and the salt spray number — Why 1.2 mm and 1.5 mm are different chairs, where rust starts on a welded frame, and what a 500 hour salt spray result actually proves.

The physics

Powder wraps a sharp edge poorly because the electrostatic field is weaker there. The 70 micron face is often 25–35 micron on an edge, and a drilled hole is thinner still.

Those are exactly the places water sits. That is why a frame can pass a coupon test on a flat plate and still rust at the first edge it has.

What helps

Deburring and a small radius on every edge before coating. The 0.5 mm radius is enough to let the powder build. It costs a pass on a linisher and nothing else.

Frames detailed this way are on hotel dining chairs, and the steel under booth seating uses the same prep.

The inspection

Take a reading on an edge and one on a face with the same gauge. The 40 micron difference means the edges are under-coated and will be the first failure.

Background in the metal guide, with metal prep before powder and salt spray, what it proves.