Salt spray proves the process, not the chair

Five hundred hours on a flat coupon is a process check. It says nothing about a crevice the coupon does not have.

25 Nov 2026 · Metal
The guide behind thisThe metal guide: wall thickness, welds and the salt spray number — Why 1.2 mm and 1.5 mm are different chairs, where rust starts on a welded frame, and what a 500 hour salt spray result actually proves.

What the test is

The scribed steel plate goes into a fog chamber at 35 °C with a salt solution. The hours are counted until red rust appears more than 2 mm from the scribe. It is a comparative test between processes, not a prediction of service life.

Which is why a 500-hour result and a frame that rusts in a year are both possible: the coupon has no weld seam, no hole, no edge radius problem.

What to ask alongside it

Film thickness on an edge, the conversion coat chemistry, and whether the coupon was taken from the same batch as the parts. Any one of those missing and the number is decoration.

Frames with the full record are on hotel dining chairs, and the same standard covers counter stools.

Where it matters

Seaside hotels, poolside, anywhere with chlorinated air. Indoors, in a heated dining room, the salt spray number is the least useful of the four things you could ask about.

This is in the metal guide, next to powder thickness and edges and metal prep before powder.

Outdoor-adjacent frames are grouped with hotel dining chairs.