Craft Notes
Home · Metal

Welding pulls a frame out of square

Heat shrinks metal as it cools, so a frame welded on one side pulls that way. The fix is a jig, not a bigger hammer.

23 Nov 2026 · Metal
The guide behind thisThe metal guide: wall thickness, welds and the salt spray number — Why 1.2 mm and 1.5 mm are different chairs, where rust starts on a welded frame, and what a 500 hour salt spray result actually proves.

Why it moves

The weld shrinks as it cools and pulls the parts toward the weld. Weld one side of a leg and the leg leans; weld four corners in sequence and the frame twists.

The 1 m frame can move 3–5 mm out of square without a jig, which is enough to make a table rock on a flat floor.

What holds it

The welding jig that clamps the frame square before the first tack. Tack in opposing pairs, weld in a balanced sequence, and let the frame cool in the jig rather than on the bench.

Frames built this way are on hotel dining tables, where a twist shows immediately as a rocking table.

The delivery check

Put the frame on a flat surface and press each corner in turn. Any rock is a frame that came out of the jig too early, and no amount of adjusting the glides fixes a twist.

This is in the metal guide, with tube shape and strength and glide types as the related notes.

Chair frames that must sit flat are on hotel dining chairs.